this post was submitted on 26 Nov 2023
15 points (100.0% liked)

3DPrinting

15338 readers
923 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

Heard I can use acetone for PLA, but not for PETG. Glued a joint and there is residue extruded and unfortunately it's a very shiny / translucent PETG. Any suggestions for cleaning up thin white residue stain from the cyanoacrylate?

top 3 comments
sorted by: hot top controversial new old
[–] thantik@lemmy.world 2 points 10 months ago

https://www.plasticsintl.com/chemical-resistance-chart

Find the one that is the most "incompatible" with acrylic, and the other one that's the most compatible with PET.

[–] stealth_cookies@lemmy.ca 2 points 10 months ago* (last edited 10 months ago) (1 children)

CA Bloom is a pain to deal with. Loctite have a few recommendations on their website. https://www.loctiteproducts.com/en/know-how/fix-stuff/remove-super-glue.html#:~:text=For%20plastic%3A%20Lay%20a%20damp,substance%20break%20down%20the%20glue.

For future reference you can get low bloom CA glues for plastics that work much better.